TYPE OF MATERIAL : nickel based alloy
PRODUCT : Inconel 601 UNS N06601 nickel based alloy seamless pipe
STANDARD : ASTM SB167
GRADE : Inconel 601 / UNS N06601 / 2.4851
Manufacturing process : The steel melt shall be refined with AOD or equivalent.
Heat Treatment : shall be supplied in the solution annealed / water quenched condition.
Surface Finish : Descaled, White Pickled, and Passivated Condition
testing facility : Accept third party testing such as SGS
2.4851 Inconel Alloy Inconel 601 Pipe UNS N06601 Nickel Based Superalloys
Inconel 601 UNS N06601 nickel based alloy seamless pipe 2.4851
Material designation: Inconel 601 nickel based alloy
US grade: N06601
German grade: 2.4851
Inconel 601 (N06601) nickel-based alloy processing heat treatment:
Inconel 601 (UNS N06601) nickel-based alloy is not a precipitation hardening alloy, so it cannot be aged hardened by heat treatment. When the temperature after cold working reaches about 900 ° C, the material softens. If the material needs high-temperature strength, it is recommended that the solution heat treatment be performed at a temperature of 1100 to 1200 ° C. At this time, the cooling method is water cooling.
Depending on the thickness of the plate, air cooling can also be used. However, in order to avoid carbide precipitation, it is recommended to cool as quickly as possible in the temperature range of 500 to 800 ° C.
Inconel 601 (N06601) nickel-based alloy chemical composition: see Table-1:
Table-1 %
| C≤ | Si≤ | Mn≤ | P≤ | S≤ | Cr≥ | Ni≥ | Mo≥ | Cu≤ |
| 0.10 | 0.50 | 1.00 | 0.020 | 0.015 | 21.0-25.0 | 72.0 | 1.00 | |
| Others | N≤ | Al≤ | Ti≤ | Fe≤ | Co≤ | V≤ | W≤ | Nb≤ |
| 1.00-1.70 | Balance |
specification:
Outer diameter Φ6—762mm; wall thickness: 0.5-50mm, maximum length 18000mm
Special specifications are available upon negotiation.

|
|